Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® YR19513 Polyolefin Wire and Cable Compound

Category Polymer , Thermoplastic , Polyolefin
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® YR19513 Polyolefin Wire and Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE YR 19513 is a colorable, thermoplastic, non-halogenated, flame retardant polyolefin compound designed for use as striping for chemically crosslinkable automotive primary and appliance wire applications.Regulatory StatusProcessingYR 19513, like other thermoplastic polyolefin compounds, can be extruded by a conventional extruder. YR 19513 crosslinks when peroxide vapors pass into the thin stripping made from this product from th4e main body of crosslinked insulation. Additionally, since the striping is on the outside surface of the insulation, it is exposed to the high temperature steam in the crosslinking process for the maximum amount of time.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.52 MPa
800 psi
Original; ASTM D638
Elongation at Break 500 %
500 %
Original; ASTM D638
Processing Properties Metric English Comments
Feed Temperature 107 - 113 °C
225 - 235 °F
Zone 2 116 - 127 °C
240 - 260 °F
Zone 3 121 - 132 °C
250 - 270 °F
Zone 4-x 121 - 132 °C
250 - 270 °F
Adapter Temperature 121 - 132 °C
250 - 270 °F
Die Temperature 121 - 132 °C
250 - 270 °F
Melt Temperature 121 - 132 °C
250 - 270 °F