Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 107 - 113 °C | 225 - 235 °F | |
LyondellBasell Petrothene® XL07407 Copolymer ApplicationsPETROTHENE XL 07407 is especially formulated for use in flame retardant, primary insulation for low voltage automotive wire and cable applications (SAE J1128), and for UL applications in.. |
|||
Feed Temperature | 107 - 113 °C | 225 - 235 °F | |
LyondellBasell Petrothene® XL07425 Copolymer ApplicationsPETROTHENE XL07425 is especially formulated for use in flame retardant primary insulation for low voltage automotive wire and cable applications (SAE J1128). Non-discoloring antioxidant .. |
|||
Feed Temperature | 107 - 113 °C | 225 - 235 °F | |
LyondellBasell Petrothene® YR19513 Polyolefin Wire and Cable Compound ApplicationsPETROTHENE YR 19513 is a colorable, thermoplastic, non-halogenated, flame retardant polyolefin compound designed for use as striping for chemically crosslinkable automotive primary and a.. |