Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 121 - 132 °C | 250 - 270 °F | |
LyondellBasell Petrothene® YR19513 Polyolefin Wire and Cable Compound ApplicationsPETROTHENE YR 19513 is a colorable, thermoplastic, non-halogenated, flame retardant polyolefin compound designed for use as striping for chemically crosslinkable automotive primary and a.. |
|||
Melt Temperature | >= 121 °C | >= 250 °F | |
Borealis Polycure™ PC780 Flame Retardant Crosslinking Polyethylene Compound for Low Voltage Insulation Polycure PC780 is a natural, chemically crosslinking polyethylene compound designed for flame retardant low voltage wire insulation and jacketing. PC780 contains a halogen-based, flame retardant ad.. |