Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® X-595A-11 is a Shore 97A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 224 °C
22 g/10 min

@Load 4.76 lb,
Temperature 435 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
ASTM D2240
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D412
Tensile Strength, Yield 13.2 MPa
1920 psi
at 100% elongation; ASTM D412
23.5 MPa
3410 psi
at 300% elongation; ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
Tear Strength 127 kN/m
728 pli
Die C; ASTM D624
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
50 %

@Temperature 70.0 °C,
Time 79200 sec
50 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Processing Properties Metric English Comments
Zone 1 185 - 195 °C
365 - 383 °F
Zone 2 190 - 200 °C
374 - 392 °F
Zone 3 195 - 205 °C
383 - 401 °F
Zone 4 195 - 205 °C
383 - 401 °F
Die Temperature 190 - 200 °C
374 - 392 °F
Descriptive Properties Value Comments
Adaptor (°C) 200-210
Users viewing this material also viewed the following: