Material Notes:
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for many types of rotary screw and piston type air compressors, hydraulic systems, blowers, and turbine oil applications. Available in Pails and DrumsInformation provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 22
22
ISO Grade
138
138
Viscosity Index
Saybolt Viscosity at 100°F 129 SUS
129 SUS
Saybolt Viscosity at 210°F 44 SUS
44 SUS
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Kinematic Viscosity at 100°C (212°F) 5.0 cSt
5.0 cSt
Thermal Properties Metric English Comments
Pour Point -56.7 °C
-70.0 °F
Flammability Test 470
470
[°F] Fire Point
>= 700
>= 700
[°F] Auto-Ignition
Flash Point 216 °C
420 °F
Descriptive Properties Value Comments
SAE No. 5W
Users viewing this material also viewed the following: