Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | |
Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance. Turbine Oil 32 is available in Drums.Information provided .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | |
Lubriplate FMO 150 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | |
Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | ASTM D445 |
Solvay Specialty Polymers FOMBLIN® M03 PFPE Lubricant Information provided by Solvay Solexis, Inc. |