Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 44 SUS
44 SUS
Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid
This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance. Turbine Oil 32 is available in Drums.Information provided ..
Saybolt Viscosity at 210°F 44 SUS
44 SUS
Lubriplate APG-75 Petroleum-Based Gear, Bearing, & Recirculating Oil
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil..
Saybolt Viscosity at 210°F 44 SUS
44 SUS
Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for..