Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | 1.67 °C | 35.0 °F | |
Lubriplate CP-8A Petroleum-Based Gear, Bearing, & Recirculating Oil This non-EP (Extreme Pressure) oil is manufactured with acidless tallow as required to meet AGMA specification 8A Comp. It is recommended for use in cone drives and double-enveloping worm gear drive.. |
|||
Pour Point | 1.67 °C | 35.0 °F | |
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |