Thermal Properties Metric English Comments
Pour Point 1.67 °C
35.0 °F
Lubriplate CP-8A Petroleum-Based Gear, Bearing, & Recirculating Oil
This non-EP (Extreme Pressure) oil is manufactured with acidless tallow as required to meet AGMA specification 8A Comp. It is recommended for use in cone drives and double-enveloping worm gear drive..
Pour Point 1.67 °C
35.0 °F
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..