Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubriplate APG-250 Petroleum-Based Gear, Bearing, & Recirculating Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate APG-250 Petroleum-Based Gear, Bearing, & Recirculating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets military specification MIL-PRF-2105E and MIL-L-21050, as well as API categories GL-3, GL-4, GL-5, and MT-1APG Series Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 100
100
Viscosity Index
680
680
ISO Grade
Saybolt Viscosity at 100°F 3700 SUS
3700 SUS
Saybolt Viscosity at 210°F 203 SUS
203 SUS
Kinematic Viscosity at 40°C (104°F) 701 cSt
701 cSt
Kinematic Viscosity at 100°C (212°F) 42 cSt
42 cSt
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flammability Test 450
450
[°F] Fire Point
Flash Point 199 °C
390 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 250
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved