Material Notes:
Bamberko® is recommended for cellulosics, polyolefins, styrenics, and PVC resins. Temperature range 350-525°F (176-275°C). Formulated to flow through injection cylinders and extrusion barrels without scratching. Recommended for use in swift color and resin changeover and to clean machines of carbonized residue. BAMBERKO® will not melt completely and are excellent for difficult purging jobs.Information provided by Claude Bamberger Molding Compounds.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 - 232 °C
350 - 450 °F
Cellulosics, Polyolefins, Styrenics & PVC Resins
204 - 288 °C
400 - 550 °F
High Temperature Engineering Plastics