Lotte Chemical Titan TITANZEX® HM5000 High density polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANZEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANZEX® HM5000 High density polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HM5000 is a high density polyethylene for extrusion monofilament. HM5000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplications: Yarns Ropes Fishing netsAdvantages: Excellent processability High stiffness High draw down capabilityInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.951 g/cc
0.0344 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 30 hour
30 hour
F<sub>50</sub>; ASTM D1693
Base Resin Melt Index 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength at Break 38.2 MPa
5540 psi
ASTM D638
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Stiffness 784.5 MPa
113800 psi
Olsen; ASTM D747
Izod Impact, Notched 1.96 J/cm
3.67 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
resin; ASTM D1525