Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® 3011 Light Cure Acrylic Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3011 Light Cure Acrylic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designed specifically for the assembly of medical devices where toxicity testing and sterilization resistance are required.Loctite® 3011 Light Cure Acrylic AdhesiveA low-viscosity, wicking UV adhesive that bonds clear plastics, metals and glass. Designed specifically for needle bonding applications. Key Substrates: Glass, metal, thermoplastic Cure Type: Ultraviolet
Physical Properties Metric English Comments
Brookfield Viscosity 100 cP

@Temperature 25.0 °C
100 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Descriptive Properties Value Comments
Color Clear/light Amber
Users viewing this material also viewed the following: