Kuraray HYBRAR® PS1 Thermoplastic Rubber-Polystyrene Blend

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber , Polystyrene (PS)
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® PS1 Thermoplastic Rubber-Polystyrene Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® and other polymers exhibit excellent vibration damping properties.Mixing Conditions: Twin screw extruder @ 200°CMolding Conditions: Injection Molding, Cylinder @ 200°C, mold @ 60°CFormulation (parts by weight): Polystyrene - 80, HYBRAR® 5127 - 20Information provided by The Kuraray Group.
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Tensile Strength, Ultimate 43.0 MPa
6240 psi
Elongation at Break 17 %
17 %
Tensile Modulus 1.863 GPa
270.2 ksi
Flexural Strength 22.0 MPa
3190 psi
Flexural Modulus 1.667 GPa
241.8 ksi
Descriptive Properties Value Comments
Loss Factor 0.068
measured by resonance method with a cantilever beam
Tan Delta 0.049
at 0°C, measured w/ Rheovibron @ 11 Hz
0.094
at 40°C, measured w/ Rheovibron @ 110 Hz
0.115
at 25°C, measured w/ Rheovibron @ 110 Hz