Polymer Property : Flexural Modulus = 1.667 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.667 GPa
241.8 ksi
Kuraray HYBRAR® PS1 Thermoplastic Rubber-Polystyrene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Flexural Modulus 1.667 GPa

@Temperature 260 °C
241.8 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po..
Flexural Modulus 1.667 GPa

@Temperature 260 °C
241.8 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS ..