Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® G1730 M (SEP) Linear Diblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G1730 M (SEP) Linear Diblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton G1730 M is a clear copolymer based on styrene and ethylene/propylene with a polystyrene content of 21%. It is supplied from North America in the physical form identified: Kraton G1730 MS - supplied as a dusted pelletKraton G1730 MO - supplied as a dusted pelletRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1730 M is used as a modifier of polymers. It is also suitable as an ingredient in formulating adhesives, sealants and coatings.Applications: Compounding and Personal Hygiene; Adhesives, Sealant and Coatings; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Melt Flow 13 g/10 min

@Load 5.00 kg,
Temperature 230 °C
13 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Ash <= 0.15 %
<= 0.15 %
For G1730 MS Silica dusted; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 61

@Time 10.0 sec
61

@Time 0.00278 hour
ASTM D2240
Descriptive Properties Value Comments
Content Dust
<0.15%, For G 1730 MO Organically dusted, KM 08
Non-staining phenolic antioxidant
0.03-0.1%, KM 08
Polystyrene
18.5-22.5%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.5%, KM 05
Styrene/Rubber Ratio 21/79
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved