Material Notes:
Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers in which the rubber monomer is a saturated olefin polymer, either ethylene/butylene or ethylene/propylene. KRATON FG polymers are functionalized versions of the G series. Available in the U.S. only. Information provided by the manufacturer, Kraton® Polymers.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.5 MPa
6600 psi
Elongation at Break 73 %
73 %
Flexural Modulus 2.03 GPa
294 ksi
Izod Impact, Notched 1.76 J/cm

@Temperature -29.0 °C
3.30 ft-lb/in

@Temperature -20.2 °F
3.2 mm (0.125 in) notch
10.57 J/cm

@Temperature 23.0 °C
19.80 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch