Karina E900D10/1-E-IS-BZ White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E900D10/1-E-IS-BZ White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.43 - 1.49 g/cc
1.43 - 1.49 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -2.14 - 0.86
-2.14 - 0.86
Color A, ME 12
-0.0200 - 2.98
-0.0200 - 2.98
Color B, ME 12
90.01 - 93.01
90.01 - 93.01
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92

@Time 15.0 sec
88 - 92

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 12.3 MPa
>= 1780 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 180 %
>= 180 %
NBR NM-IEC 60811-1-1
Descriptive Properties Value Comments
Application Helix Hose