Material Notes:
PVC Compound with NBR; recommended for injection of automotive parts and extrusion of flexible jacket for electrical cables.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.25 - 1.29 g/cc
1.25 - 1.29 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -1.36 - -1.20
-1.36 - -1.20
Color B, ME 12
-0.870 - -0.710
-0.870 - -0.710
Color A, ME 12
26.69 - 26.85
26.69 - 26.85
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 350 %
>= 350 %
NBR NM-IEC 60811-1-1
Descriptive Properties Value Comments
Application Automotive