Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.86 MPa @Strain 100 % |
1140 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180 is a 80 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2180 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength | 7.86 MPa @Strain 100 % |
1140 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180G is a 80 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2180G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength | 7.86 MPa @Strain 100 % |
1140 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 3180G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 3180G is a non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 3180G can be used for extrusion and injection molding healthcare applications. This pr.. |
|||
Tensile Strength | 7.86 MPa @Strain 100 % |
1140 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3856 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E TR 500D22/173 Honey PVC Compound Honey PVC compound additivated with nitrile rubber, recommended for injection of general soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | NBR NM-IEC 60811-1-1 |
Karina E TR-652D48/1-B-IS Black PVC Compound PVC Compound with NBR; recommended for injection of automotive parts and extrusion of flexible jacket for electrical cables.Information provided by Karina Indústria e Comércio de Plásticos .. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina FADA 45-YAT White PVC Compound Non-toxic PVC compound recommended for injection of inseminator for veterinary applicationsInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D32/13-AT-IS Orange PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D35/1-AT-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D42/10-AT-IS Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 603-48/1-Y-BZ Black PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 650D08/244-D-IS Beige PVC Compound Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 650D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 651-48/1-B-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for extrusion and injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 752-12/6-Y-BZ Ruby Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 52/205-D-AT-IS Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 650D48/1 Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 670D10/116-Y White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 670D35/1-A-AT-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 680D48/1-G-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 801D06/418-C Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 600D48/1-C-IS Black PVC Compound PVC Compound recommended for injection of automotive parts and extrusion of flexible jacket for electrical cablesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 7.85 MPa | 1140 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well .. |
|||
Tensile Strength | 7.86 MPa | 1140 psi | Silicone Property; ASTM D412 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Tensile Strength | 7.86 MPa | 1140 psi | Silicone Property; ASTM D412 |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Tensile Strength | 7.86 MPa | 1140 psi | Silicone Property; ASTM D412 |
Arlon 44602W020W 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1165 FiberglassProduct is designed to meet the FAR 25.853 App.F, P.1,.Aii flame resistance requirements b.. |