Karina E 911D40/77-IS Green PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 911D40/77-IS Green PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.23 - 1.29 g/cc
1.23 - 1.29 g/cc
ASTM D 792
ASTM Color -58.95 - -55.95
-58.95 - -55.95
Color A, ME 12
4.19 - 7.19
4.19 - 7.19
Color B, ME 12
72.72 - 75.72
72.72 - 75.72
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92

@Time 15.0 sec
88 - 92

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 14.7 MPa
>= 2130 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Hoses