Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL T 161B Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 161B Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 161B is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 161B is a block copolymer with radial molecular structure, providing excellent mechanical properties, high strength and elasticity in a wide range of formulated products.Main Applications: Used in bitumen modification in waterproofing membranes, road pavement and pipe coating applications. Also used as a high strength base in formulated compounds for footwear and technical applications, the grade could be suitable for adhesives and plastic modification.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Brookfield Viscosity 2.0 cP
2.0 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
300% Modulus 0.00250 GPa
0.363 ksi
ASTM D412