Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E 801D06/418-C Blue PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 801D06/418-C Blue PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.39 g/cc
1.33 - 1.39 g/cc
ASTM D 792
ASTM Color -32.38 - -29.38
-32.38 - -29.38
Color B, ME 12
0.99 - 3.99
0.99 - 3.99
Color A, ME 12
46.37 - 49.37
46.37 - 49.37
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 150 %
>= 150 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts
Copyright © lookpolymers.com All Rights Reserved