Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina CAK 751-48/1-TEC-IS Black PVC Compound

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina CAK 751-48/1-TEC-IS Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reclaimed PVC compound, recommended for plug injection.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.43 g/cc
1.37 - 1.43 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77

@Time 15.0 sec
73 - 77

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 9.81 MPa
>= 1420 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application Plugs
Users viewing this material also viewed the following: