Karina 601D10/1-A White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 601D10/1-A White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.23 - 1.29 g/cc
1.23 - 1.29 g/cc
ASTM D 792
ASTM Color -1.76 - 1.24
-1.76 - 1.24
Color A, ME 12
-0.0400 - 2.96
-0.0400 - 2.96
Color B, ME 12
88.13 - 91.13
88.13 - 91.13
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 5.88 MPa
>= 853 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Soles