Tensile Strength >= 5.88 MPa
>= 853 psi
ASTM D 638
Karina E CAK 65 Ivory PVC Compound
Reclaimed PVC compound, recommended for injection of footwear soles. Color it is not guaranteed. CAK = alternative compound.Information provided by Karina Indústria e Comércio de Plástico..
Tensile Strength >= 5.88 MPa
>= 853 psi
ASTM D 638
Karina 550-48/1-C-IS Black PVC Compound
Heavy metal free PVC compound recommended for technical parts extrusion and injection.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 5.88 MPa
>= 853 psi
ASTM D 638
Karina 601D10/1-A White PVC Compound
For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 5.88 MPa
>= 853 psi
ASTM D 638
Karina E 650D35/1-A Ivory PVC Compound
For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.