Polymer Property : Bulk Density = 0.368 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.368 g/cc
0.0133 lb/in³
loose
Nyco NYAD® G Special Wollastonite
Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite ..
Bulk Density 0.368 - 0.449 g/cc
0.0133 - 0.0162 lb/in³
Loose
KaMin KaMin® 70C Kaolin Clay - Calcined
High brightness, work-horse calcined kaolin clay, extremely low crystalline silica content.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Mat..
Bulk Density 0.368 - 0.449 g/cc
0.0133 - 0.0162 lb/in³
Loose
KaMin Polyfil® 70 Kaolin Clay - Calcined
Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due ..
Bulk Density 0.368 - 0.449 g/cc
0.0133 - 0.0162 lb/in³
Loose
KaMin Polyfil® 80 Kaolin Clay - Calcined
Higher brightness, medium particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber GoodsInformation provided by KaMin LLC.
Bulk Density 0.368 g/cc
0.0133 lb/in³
Loose
CIMBAR CIMTUFF® 9107 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Bulk Density 0.368 g/cc
0.0133 lb/in³
Loose
CIMBAR Gel Talc for Polyester Filler
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes..
Bulk Density 0.368 g/cc
0.0133 lb/in³
Loose
CIMBAR MV 607 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..
Bulk Density 0.368 g/cc
0.0133 lb/in³
Loose
CIMBAR RP 9305 Talc
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R..