Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Yield 26 %
26 %
ASTM D638
1% Secant Modulus 2200 MPa
319000 psi
ASTM D790A
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648