Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Intercontinental Polymers 1128 Bicomponent PBT/PET Fiber Type - 1.8 Denier X 3 Inches

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polyethylene Terephthalate (PET)
Manufacturer Intercontinental Polymers, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers 1128 Bicomponent PBT/PET Fiber Type - 1.8 Denier X 3 Inches.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50/50 PBT Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenier fabrics, synthetic suede fabrics and wipes, automobile headliners.Information provided by Intercontinental Polymers.
Mechanical Properties Metric English Comments
Elongation at Break 55 - 85 %
55 - 85 %
LFL-09
Tenacity 0.274 - 0.344 N/tex
3.10 - 3.90 g/denier
LFL-09
Thermal Properties Metric English Comments
Melting Point 200 - 300 °C
392 - 572 °F
Sheath Melt Point; LCL-PR29
Shrinkage 0.00 - 6.0 %
0.00 - 6.0 %
Hot Air Shrinkage; LFL-07
Descriptive Properties Value Comments
Chip Weight 0.8 - 1.4 g/50 chips
LCL-PR06
Crimp/Inch 15 - 21
LFL-03
Finish 0.1 - 0.3%
LCL-PR39