Gwent Electronic Materials C2050830D8 80:20 Silver Palladium Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2050830D8 80:20 Silver Palladium Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C2050830D8 is an ink based on a 80:20 ratio of Silver:Palladium. It is designed for use in Single Layer PZT applications. This ink can be used in both dip and hand soldering. This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester. 180-340 meshSubstrate: Multilayer or Single layer PZT tapes and foilsInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 59.5 - 60.5 %

@Temperature 800 °C
59.5 - 60.5 %

@Temperature 1470 °F
Viscosity 12000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
12000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 9.00 microns
0.354 mil
Fired thickness, printed through 325ss mesh
Storage Temperature 20.0 °C
68.0 °F
sealed container
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 10.0 MPa
>= 1450 psi
on Alumina substrate
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.017 ohm
0.017 ohm
Processing Properties Metric English Comments
Sintering Temperature 850 - 1150 °C
1560 - 2100 °F
Cure Time 15.0 min

@Temperature 150 °C
0.250 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month