Ineos L34N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos L34N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.
Physical Properties Metric English Comments
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790B
Izod Impact, Notched 0.481 J/cm

@Temperature -20.0 °C
0.900 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
1.33 J/cm

@Temperature 23.0 °C
2.50 ft-lb/in

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved