Polymer Property : Liquidus = 320 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 160 °C
320 °F
Indium Corp. Indalloy 93 Bismuth-Lead Solder Alloy
Information Provided by Indium Corporation
Liquidus 160 °C
320 °F
Indium Corp. Indalloy 94 Lead-Tin-Cadmium Solder Alloy
Information Provided by Indium Corporation