Material Notes:
Very good resistance to alkaline corrosionInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.42 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 10.2

@Load 100 kg,
Time 30.0 sec
10.2

@Load 220 lb,
Time 0.00833 hour
Tensile Strength at Break 36.3 MPa
5260 psi
Elongation at Break 101 %
101 %
Shear Strength 29.6 MPa
4300 psi
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 23.0 W/m-K

@Temperature 85.0 °C
160 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 134 - 181 °C
273 - 358 °F
Solidus 134 °C
273 °F
Liquidus 181 °C
358 °F
Component Elements Properties Metric English Comments
Indium, In 25 %
25 %
Lead, Pb 37.5 %
37.5 %
Tin, Sn 37.5 %
37.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000220 ohm-cm
0.0000220 ohm-cm