Polymer Property : Shear Strength = 4300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 29.6 MPa
4300 psi
Indium Corp. Indalloy 5 Indium-Lead-Tin Solder Alloy
Very good resistance to alkaline corrosionInformation Provided by Indium Corporation
Shear Strength 29.6 MPa

@Temperature 21.0 °C
4300 psi

@Temperature 69.8 °F
Overlap
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b..
Shear Strength 29.6 MPa

@Temperature 218 °C
4300 psi

@Temperature 424 °F
Bond Line
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M