Solidus 134 °C
273 °F
Indium Corp. Indalloy 139 Lead Free Solder Alloy
Information Provided by Indium Corporation
Solidus 134 °C
273 °F
Indium Corp. Indalloy 5 Indium-Lead-Tin Solder Alloy
Very good resistance to alkaline corrosionInformation Provided by Indium Corporation
Solidus 134 °C
273 °F
Williams Advanced Alloys WS181 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys