Indium Corp. Indalloy 34 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 34 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.70 g/cc
0.350 lb/in³
Thermal Properties Metric English Comments
Melting Point 83.0 - 92.0 °C
181 - 198 °F
Solidus 83.0 °C
181 °F
Liquidus 92.0 °C
198 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 52 %
52 %
Cadmium, Cd 1.0 %
1.0 %
Lead, Pb 31.7 %
31.7 %
Tin, Sn 15.3 %
15.3 %