Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.70 - 9.90 g/cc | 0.350 - 0.358 lb/in³ | |
MarkeTech Cu/Mo/Cu 1:4:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Density | 9.69 g/cc | 0.350 lb/in³ | |
Indium Corp. Indalloy 257 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.70 g/cc | 0.350 lb/in³ | |
Indium Corp. Indalloy 34 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.70 g/cc | 0.350 lb/in³ | |
Indium Corp. Indalloy 37 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.70 - 10.1 g/cc | 0.350 - 0.365 lb/in³ | |
H.C. Starck MoCu 80/20 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |