Indium Corp. Indalloy 114 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 114 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Thermal Properties Metric English Comments
Melting Point 183 - 205 °C
361 - 401 °F
Solidus 183 °C
361 °F
Liquidus 205 °C
401 °F
Component Elements Properties Metric English Comments
Lead, Pb 15 %
15 %
Tin, Sn 85 %
85 %