Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.02 g/cc
0.290 lb/in³
Thermal Properties Metric English Comments
Melting Point 62.0 °C
144 °F
Eutectic
Solidus 62.0 °C
144 °F
Liquidus 62.0 °C
144 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 30.8 %
30.8 %
Cadmium, Cd 7.5 %
7.5 %
Indium, In 61.7 %
61.7 %