Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.02 g/cc | 0.290 lb/in³ | |
Indium Corp. Indalloy 18 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.02 g/cc | 0.290 lb/in³ | |
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability .. |
|||
Density | 8.02 g/cc | 0.290 lb/in³ | |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Density | 8.02 g/cc | 0.290 lb/in³ | |
Special Metals NIMONIC® Alloy PE11 A nickel-iron-chromium alloy precipitation hardened by titanium and aluminum and solid-solution strengthened by an addition of molybdenum. It was developed as a high-strength sheet alloy for use at.. |
|||
Density | 8.02 g/cc | 0.290 lb/in³ | |
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |
|||
Density | 8.02 g/cc | 0.290 lb/in³ | |
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy Uses: Pressure vessels, pumps, valves, HX tubing and piping for the CPI and HPI. Trays, flanges, fasteners, wire, screens.Property values are for samples in the metallurgical condition: 2050°F age... |
|||
Density | 8.02 g/cc | 0.290 lb/in³ | |
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |