Indium Corp. Indalloy 13 Indium Solder Alloy

Category Metal , Nonferrous Metal , Indium Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 13 Indium Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.63 g/cc
0.276 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 4.0
4.0
Tensile Strength at Break 10.18 MPa
1476 psi
Shear Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 39.0 W/m-K

@Temperature 85.0 °C
271 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 125 °C
257 °F
Solidus 125 °C
257 °F
Liquidus 125 °C
257 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 5.4 %
5.4 %
Indium, In 70 %
70 %
Lead, Pb 9.6 %
9.6 %
Tin, Sn 15 %
15 %