Indium Corp. 2036 Non-Activated Rosin Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 2036 Non-Activated Rosin Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2036 is a non-activated rosin flux blended with pure alcohol and water white rosin. This flux is best suited for easy to solder applications where high-reliability of the assembly is the highest priority.FeaturesLeaves an insulative and benign residue.Best for use in high-reliability applications without removalProvides good solderabilityPhysical PropertiesColor: AmberFlux Type: R0L0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.869 g/cc

@Temperature 25.0 °C
0.869 g/cc

@Temperature 77.0 °F
0.874 g/cc

@Temperature 15.5 °C
0.874 g/cc

@Temperature 59.9 °F
Solids Content 36.42 %
36.42 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC