Material Notes:
Kingsley is a coarse-grained, white firing kaolin used in the dinnerware, tile, artware and electrical porcelain industries.Information provided by Imerys
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
25% finer than
1.0 µm
1.0 µm
44% finer than
2.0 µm
2.0 µm
58% finer than
5.0 µm
5.0 µm
80% finer than
10 µm
10 µm
91% finer than
20 µm
20 µm
97% finer than
Particle Mesh Size 325 Mesh
325 Mesh
2.5% retained
pH 5.5
5.5
Specific Surface Area 12.5 m²/g
12.5 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00190 GPa
0.275 ksi
dry
Component Elements Properties Metric English Comments
Al2O3 38.4 %
38.4 %
CaO 0.10 %
0.10 %
Carbon, C 0.030 %
0.030 %
Fe2O3 0.40 %
0.40 %
K2O 0.10 %
0.10 %
Loss on Ignition(%) 13.6 %
13.6 %
MgO 0.10 %
0.10 %
Na2O 0.10 %
0.10 %
SiO2 44.8 %
44.8 %
Sulfur, S 0.040 %
0.040 %
TiO2 1.6 %
1.6 %
Descriptive Properties Value Comments
M.B.I. (meq/100g) 3.3