Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICORENEâ„¢ 110-1081 LMDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 110-1081 LMDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ICORENE 110-1081 polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface porosity and good overall properties. This product is enhanced with ICOPower and OptiFlo. The base resin is FDA approved and is fully stabilized to UV8 level. Key Characteristics: fast processing, low pinholing, wide processing window. Applications: This ICORENE® grade is particularly suitable for use in toy applications. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 190 °C
14 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength, Yield 16.10 MPa
2335 psi
2"/min; ASTM D638
Elongation at Break 416 %
416 %
2"/min; ASTM D638
Flexural Modulus 0.6200 GPa
89.92 ksi
ASTM D790