Material Notes:
Approx. H+ equivalent weight 95. Mix Ratio with GY 6010 is 50.Comments/Applications: Low viscosity polyamidoamine for solvent free systems. Good mechanical properties. Adhesives, sealants, flooring and coatings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 250 - 500 cP
250 - 500 cP
Processing Properties Metric English Comments
Pot Life 75 min
75 min