Huntsman Euredur 450 Cycloaliphatic Amine

Category Polymer , Thermoset , Epoxy , Epoxy, Cycloaliphatic, Molded
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Euredur
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Euredur 450 Cycloaliphatic Amine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: For high-humid application areas and underwater applications. To be used in surface tolerant coatings systems.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1000 - 2000 cP
1000 - 2000 cP
Processing Properties Metric English Comments
Pot Life 60 min
60 min