Material Notes:
Description: Capran® 980 is a clear (low haze level), heat-stabilized cast film produced from modified nylon 6 resin. Capran® 980 has excellent heat stability and resistance to pinholing. It can be used at temperatures up to 390°F (199°C) for typical composite cure cycle times. Applications: Capran® 980 is recommended as bagging film for advanced composite fabrication and other high temperature applications where dimensional stability, adherence to sealant tapes and uniform film gauge are essential. Information provided by Honeywell.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0410 lb/in³
Yield Density
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa
16000 psi
ASTM D882
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D882
Elongation at Break 375 %
375 %
ASTM D882
Tear Strength Test 45
45
grams/mil; ASTM D1922
Thermal Properties Metric English Comments
Melting Point 218 - 220 °C
424 - 428 °F
crystalline melting point; Hot Stage Microscope
Shrinkage <= 2.00 %

@Temperature 149 °C,
Time 1800 sec
<= 2.00 %

@Temperature 300 °F,
Time 0.500 hour
ASTM D1204