Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexWeb® HRH-78 - 3/16 - 6.0 Commercial Grade Nomex Honeycomb/Phenolic Resin

Category Polymer , Thermoset , Phenolic
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-78 - 3/16 - 6.0 Commercial Grade Nomex Honeycomb/Phenolic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding, the block is dipped in a phenolic resin. After curing the resin, slices are cut to the desired thickness. Using this process, a wide range of cell sizes, paper thicknesses, and densities can be produced. An OX-Core confiation featuring enhanced formability is available upon request.Features: High strength at low densities; Small cell sizes at low densities; Damage resistant under normal shop use; Formable; Flame resistant; Good bonding surfaces; Good thermal and electrical insulator.Applications: HexWeb HRH-78 was developed by Hexcel to offer most of the characteristics of HexWeb HRH-10 for exclusive use in non-aerospace applications, such as pleasure boats, skis, surfboards, ground antennas, and navy joiner panels.
Physical Properties Metric English Comments
Density 0.0961 g/cc
0.00347 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength 7.067 MPa
1025 psi
Bare
7.58 MPa
1100 psi
Stabilized
Shear Modulus 0.0379 GPa
5.50 ksi
Plate Shear, W Direction, preliminary value obtained from limited testing
0.0896 GPa
13.0 ksi
Plate Shear, L Direction, preliminary value obtained from limited testing
Shear Strength 1.62 MPa
235 psi
Plate Shear, W Direction
3.10 MPa
450 psi
Plate Shear, L Direction
Users viewing this material also viewed the following: