Henkel Hysol Benzoxazine 99120 Infusion Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Henkel
Trade Name Hysol Benzoxazine
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol Benzoxazine 99120 Infusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part Infusion resin for VARTM processing. Moderate viscosity, very high toughness with good hot wet properties.
Physical Properties Metric English Comments
Storage Temperature 23.0 °C
73.4 °F
Mechanical Properties Metric English Comments
Tensile Strength 97.0 MPa
14100 psi
Elongation at Break 4.6 %
4.6 %
Tensile Modulus 0.00370 GPa
0.537 ksi
Flexural Modulus 0.00350 GPa

@Temperature 25.0 °C
0.508 ksi

@Temperature 77.0 °F
Flexural Stiffness 146 MPa

@Temperature 25.0 °C
21200 psi

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 180 °C
1.50 hour

@Temperature 356 °F
Descriptive Properties Value Comments
Consistency Moderate Viscosity
Form 1 part
Fracture Toughness (J/m2) 471
Pot Life 6 months