Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00370 GPa | 0.537 ksi | |
Henkel Hysol Benzoxazine 99120 Infusion Resin One-part Infusion resin for VARTM processing. Moderate viscosity, very high toughness with good hot wet properties. |